Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 284.7 J @Treatment Temp. 204 °C |
210.0 ft-lb @Treatment Temp. 400 °F |
tempered at 350°F |