Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 203 J | 150 ft-lb | |
CMW® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |