Polymer Property : Charpy Impact, Unnotched = 140 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 140 J
103 ft-lb
1/2 size bar
Kinetics MIM 17-4PH Stainless Steel (H1100 Condition)
Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat..