Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.752 GPa | 979.3 ksi | tangent; ASTM D790 |
Diamond Polymers NPP30-0800 GF40 40% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |