Polymer Property : Flexural Modulus = 9510 ksi
Polymer Property :
Flexural Modulus =
9510 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
65.6
GPa
9510
ksi
EN2562
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K
Fiber: HS Carbon, Plain Weave, 193 g/m2Information provided by HexCel