Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.468 GPa | 938.1 ksi | ASTM D790 |
Kolon KOCETAL® GF305 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Flexural Modulus | 6.468 GPa | 938.1 ksi | ASTM D790 |
Kolon KOCETAL® GF705 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffnessApplications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |