Polymer Property : Flexural Modulus = 930 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.74 - 6.41 GPa
397 - 930 ksi
Average value: 4.02 GPa Grade Count:19
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..