Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.635 GPa | 92.1 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1008 LMDPE Rotational Molding Resin Description: ICORENE 115-1008 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Flexural Modulus | 0.635 GPa | 92.1 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1650 LMDPE Rotational Molding Resin Description: ICORENE 115-1650 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Flexural Modulus | 0.635 GPa | 92.1 ksi | ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-1653 LMDPE Rotational Molding Resin Description: ICORENE 115-1653 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |