Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 900.3 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.207 GPa
900.3 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 4003 RC 40% Glass Filled Polypropylene
Multi-Pro 4003 RC is a chemically coupled glass reinforced polypropylene compound suitable for engineered plastics applications due to its high heat, flexural and impact properties.Data provided by ..
Flexural Modulus 6.207 GPa
900.3 ksi
ASTM D-790
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Flexural Modulus 6.207 GPa
900.3 ksi
ASTM D790
Lucent Polymers LPB-130 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.