Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.61 GPa | 1390 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 9.61 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific) LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat. |
|||
Flexural Modulus | 9.61 GPa | 1390 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |