Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.800 - 9.26 GPa | 116 - 1340 ksi | Average value: 2.56 GPa Grade Count:16 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |