Polymer Property : Flexural Modulus = 883 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.09 GPa
883 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX06411H PC
LNP* THERMOCOMP* DX06411H is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.