Mechanical Properties Metric English Comments
Flexural Modulus 0.6009 GPa
87.15 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 115-1333 LMDPE Rotational Molding Resin
Description: ICORENE 115-1333 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene..