Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.646 GPa | 818.9 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY DF2049 PC LNP* LUBRILOY* DF2049 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Wear Resistant, Flame Retardant. |