Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.565 GPa | 81.9 ksi | ASTM D790 |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |