Polymer Property : Flexural Modulus = 8.75 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.75 GPa
1270 ksi
Plastcom SLOVAMID 6/66 GF 30 FRG 5 TS PA6/66, 30% glass fibre, flame retardant
FeaturesPA 6 + PA 66 alloy for injection moulding, chemically reinforced with 30 % glass fibre, with halogen and phosphorus free flame retardant. Main features: flammability in accordance with UL 94..
Flexural Modulus 8.75 GPa
1270 ksi
ISO 178
Radici Radiflam® ARV350 AF (dry) Nylon 66
PA66 Self-extinguishing glass-fiber reinforced with phosphorousInformation provided by Radici group.
Flexural Modulus 8.75 GPa
1270 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC
LNP THERMOCOMP* DF006ER is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 8.75 GPa
1270 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS
LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
Flexural Modulus 8.75 GPa
1270 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific)
35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
Flexural Modulus 8.75 GPa
1270 ksi
STN EN ISO 178
Plastcom SLOVAMID 66/6 GF 30 Polyamide 66/6, 30% Glass Fiber  (discontinued **)
FeaturesChemically reinforced alloy PA 66 and PA 6 with 30% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and el..