Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.532 GPa
1237 ksi
ASTM D790
Kolon KOPA® KN333G30BL G/F Reinforced Nylon 66
G/F 30% reinforcedApplications Engine coversInformation provided by API-Kolon.
Flexural Modulus 8.532 GPa
1237 ksi
ASTM D790
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66
Oil resistantApplications Surge tanksInformation provided by API-Kolon.