Polymer Property : Flexural Modulus = 8.129 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.129 GPa
1179 ksi
ASTM D790
PlastxWorld CEVIAN® A5626 30% GF PA/ABS Alloy, DAM
Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.