Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.500 GPa | 797.7 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1010G20FRMA Polycarbonate, 20% Glass Filled Polycarbonate, 20% Glass Filled, Flame RetardantInformation provided by Ravago. |