Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.42 GPa | 786 ksi | ASTM D790 |
PlastxWorld CEVIAN® S1220 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |