Polymer Property : Flexural Modulus = 763 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.26 GPa
763 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific)
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Flexural Modulus 5.26 GPa
763 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.