Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 76.5 GPa @Temperature 25.0 °C |
11100 ksi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |