Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 51.7 GPa @Temperature 22.8 °C |
7500 ksi @Temperature 73.0 °F |
ASTM D790 |
Quadrant EPP Ketron® LSG CC PEEK Ketron PEEK with 57% Woven Carbon Fiber |
|||
Flexural Modulus | 51.7 GPa | 7500 ksi | |
Greene Tweed Xycomp® 1030-02 Carbon/Nylon 12 Composite Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |