Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.500 - 0.500 GPa @Temperature 90.0 - 90.0 °C |
72.5 - 72.5 ksi @Temperature 194 - 194 °F |
Average value: 0.500 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |