Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.95 GPa | 718 ksi | |
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Flexural Modulus | 4.95 GPa | 718 ksi | |
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Flexural Modulus | 4.95 GPa | 718 ksi | ISO 178 |
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |