Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.14 - 7.85 GPa | 310 - 1140 ksi | Average value: 2.65 GPa Grade Count:14 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Modulus | 1.50 - 7.85 GPa | 218 - 1140 ksi | Average value: 4.04 GPa Grade Count:36 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |