Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0530 GPa | 7.69 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-720 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength p.. |
|||
Flexural Modulus | 0.0530 GPa @Temperature 49.0 °C |
7.69 ksi @Temperature 120 °F |
ASTM D790 |
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |