Polymer Property : Flexural Modulus = 7.45 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 7.45 GPa
1080 ksi
1.3 mm/min; ASTM D790
PolyOne Edgetek® AS-30GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS)
Information provided by PolyOne
Flexural Modulus 7.45 GPa
1080 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66
LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant.
Flexural Modulus 7.45 GPa
1080 ksi
ASTM D790
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Flexural Modulus 7.45 GPa
1080 ksi
Shinil Chemical SHINSTRA PA-6 AG30N Structural Polymer Wheel Cover
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Flexural Modulus 7.45 GPa
1080 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS
LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am..
Flexural Modulus 7.45 GPa
1080 ksi
ASTM D790
PlastxWorld CEVIAN® S1230 PC/ABS alloy
Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Modulus 7.45 GPa

@Temperature 90.0 °C
1080 ksi

@Temperature 194 °F
ASTM D790
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..