Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.81 GPa | 698 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |