Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.76 - 4.80 GPa | 400 - 696 ksi | Average value: 3.88 GPa Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |