Flexural Modulus 47.6 GPa
6900 ksi
Greene Tweed Xycomp® 1030-01 Carbon/Nylon 12 Composite
Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st..