Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.276 - 0.480 GPa | 40.0 - 69.6 ksi | Average value: 0.346 GPa Grade Count:11 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |
|||
Flexural Modulus | 0.200 - 0.480 GPa | 29.0 - 69.6 ksi | Average value: 0.287 GPa Grade Count:5 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |