Polymer Property : Flexural Modulus = 674.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.647 GPa
674.1 ksi
UNI EN ISO 14125: 2000
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
Processed by selective laser sintering (SLS). Windform® SP is a deep black composite polyamide that is a “Top” level material within the polyamide Windform® materials for additive manufacturing..