Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.500 GPa | 652.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339G20M10CL Glass/Mineral Reinforced Coupled |
|||
Flexural Modulus | 4.500 GPa | 652.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339M30CL Mica Reinforced Coupled |