Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.32 GPa | 627 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Flexural Modulus | 4.32 GPa | 627 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead. |
|||
Flexural Modulus | 4.32 GPa | 627 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12 4.3 specific gravity nylon 12, clean compound system |
|||
Flexural Modulus | 4.32 GPa | 627 ksi | ASTM D790 |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |