Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.300 GPa | 623.6 ksi | ASTM D790 |
Aclo Accutech Polyethylene HD0234G40UVL High Density Glass Reinforced UV Stabilized |
|||
Flexural Modulus | 4.300 GPa | 623.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T40L1 Talc Reinforced |
|||
Flexural Modulus | 4.300 GPa | 623.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336W40L1 Wollastonite Reinforced |