Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.17 GPa | 604 ksi | ASTM D790 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |