Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 41.4 GPa | 6000 ksi | ASTM D790 |
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement