Polymer Property : Flexural Modulus = 6.99 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0344 - 0.0482 GPa
4.99 - 6.99 ksi
Secant 1%; ASTM D-790-95
Multibase Multi-Flex® TPO DEFA 1047
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.