Mechanical Properties Metric English Comments
Flexural Modulus 0.0480 GPa
6.96 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App..
Flexural Modulus 0.0480 GPa
6.96 ksi
ASTM D790
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0480 GPa

@Thickness 2.00 mm
6.96 ksi

@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
BASF Elastollan® C85A10 (917) Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.