Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.906 GPa | 1002 ksi | ASTM D790 |
E-Polymers SEPAZ® V220A 20% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |