Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.72 GPa | 975 ksi | ASTM D790 |
Omni Plastics OmniTech™ HDPE GRC40 Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Flexural Modulus | 6.72 GPa | 975 ksi | ISO 178 |
Polyplastics Duranex® CRN7015 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 6.72 GPa | 975 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10 LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive. |