Flexural Modulus 6.55002 - 6.55002 GPa

@Temperature 149 - 149 °C
950.015 - 950.015 ksi

@Temperature 300 - 300 °F
Average value: 6.55 GPa Grade Count:1
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..