Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.491 GPa | 941.4 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Flexural Modulus | 6.491 GPa | 941.4 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific) LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b.. |