Mechanical Properties Metric English Comments
Flexural Modulus 6.4088 GPa
929.52 ksi
ASTM D790
Ecomass® 1080TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..