Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.3765 GPa | 924.83 ksi | ASTM D790 |
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Flexural Modulus | 6.3765 GPa | 924.83 ksi | ASTM D790 |
E-Polymers SEPAZ® LH30 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |