Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.345 GPa | 920.3 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 4008 RC Medium Impact 40% Glass Filled Polypropylene Multi-Pro 4008 RC is a chemically coupled glass reinforced polypropylene compound exhibiting highest flexural modulus, flex strength and high impact resistance. Heat resistance is high due to highl.. |