Flexural Modulus 0.0371 - 0.0433 GPa
5.38 - 6.28 ksi
Average value: 0.0396 GPa Grade Count:3
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..