Polymer Property : Flexural Modulus = 6.22 GPa
Polymer Property :
Flexural Modulus =
6.22 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
6.22
GPa
902
ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl PX7446 PPE+PS
This data was supplied by SABIC-IP for the Americas region.