Polymer Property : Flexural Modulus = 6.2069 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.2069 GPa
900.24 ksi
ASTM D790
Lucent Polymers GPB-130L Polybutylene Terephthalate, 30% Glass Fiber Reinforced
Recycled ContentAdd "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Flexural Modulus 6.2069 GPa
900.24 ksi
ASTM D790
Lucent Polymers GPP-240 Homopolymer Polypropylene, 40% Glass Fiber Reinforced, Chemically Coupled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 6.2069 GPa
900.24 ksi
ASTM D790
Lucent Polymers L6-140 Nylon 6, 15% Glass Fiber and 25% Mineral Reinforced
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.